Search by Substrate

Shot Glass Sublimation Instructions

Varies by Method

Varies by Method

Varies by Method

OUR INSTRUCTIONS ARE BASED ON USING A DK20S, DK3110 AND/OR A COUNTER TOP CONVECTION OVEN. TIMES AND TEMPERATURES WILL VARY DEPENDING ON WHICH EQUIPMENT YOU USE.


Detailed Instructions

Substrate SHOT04, SHOT01, DECO-SHOT01K, SHOT25, SHOT26, SHOT27, SHOT29, SHOT30
Temperature Varies by Method
Time (min:sec) Varies by Method
Pressure Varies by Method
Additional Heat Tape
Recommended Paper DyeTrans Multi-Purpose or TexPrint
Heat Press Instructions

Hover transfer under open heat press for 10 seconds to dry excess moisture.

Shrink Wrap Instructions Instructions for Using an Oven and SubliShrink

Time: 8 Minutes
Temp: 400°

1. Remove all lids or plastic parts.
2. Secure image to substrate using heat tape.
3. Place SubliShrink around blank, secure with tape if necessary.
4. Use heat gun to form SubliShrink evenly around blank product.
5. Place in oven for appropriate time and temperature.

Pressure Cheat Sheet

Contact Level
PSI
Press Dial Level
Average Human Resistance Felt
Contact Pressure
10-15 psi
1 on press dial
where the platen just makes physical contact with product
Light Pressure
20 psi
2 on press dial
resistant with one arm pressing down, easy with two arms
Medium Pressure
40-60 psi
3-5 on press dial
resistant with two arms pressing down, doesn’t require usage of shoulders
Heavy Pressure
80 psi
6 and up on dial
very resistant with two arms pressing down, requires lifting of elbows and shoulders to lock in place