Search by Substrate

Stainless Steel Mug Sublimation Instructions

Varies by Method

Varies by Method

Varies by Method

OUR INSTRUCTIONS ARE BASED ON USING A DK20S, DK3110 AND/OR A COUNTER TOP CONVECTION OVEN. TIMES AND TEMPERATURES WILL VARY DEPENDING ON WHICH EQUIPMENT YOU USE.


Detailed Instructions

Substrate SSMUG15-W
Temperature Varies by Method
Time (min:sec) Varies by Method
Pressure Varies by Method
Additional
Recommended Paper
Heat Press Instructions

Hover transfer under open heat press for 10 seconds to dry excess moisture.

Mug Press Instructions:
1. Secure transfer to the Mug using Heat Tape.
2. Surrond with protective paper.
3. Place Mug in Mug Press.
4. Press for 2 minutes at 375°.
Oven Instructions Oven Instructions:
1. Affix design to mug using heat tape
2. Cover mug with protective paper
3. Place DYEWRAP05 around mug
4. Place in oven for 10 minutes at 375°
5. Remove from oven
6. Remove DYEWRAP from mug
7. Place on Koolplate or fan to cool
Shrink Wrap Instructions Instructions for Using an Oven and SubliShrink

360° 6 Minutes

1. Remove all plastic parts and lids
2. Cut out design and affix to tumbler using heat tape
3. Place in shrink bag
4. Use heat gun to shrink bag to tumbler
5. Place in oven for 6 minutes at 360°
6. Remove from oven
7. Remove shrink bag and image from tumbler

Pressure Cheat Sheet

Contact Level
PSI
Press Dial Level
Average Human Resistance Felt
Contact Pressure
10-15 psi
1 on press dial
where the platen just makes physical contact with product
Light Pressure
20 psi
2 on press dial
resistant with one arm pressing down, easy with two arms
Medium Pressure
40-60 psi
3-5 on press dial
resistant with two arms pressing down, doesn’t require usage of shoulders
Heavy Pressure
80 psi
6 and up on dial
very resistant with two arms pressing down, requires lifting of elbows and shoulders to lock in place
Report a Problem